MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan Sheen Soon Sheenthane® AH-560 TPU for Hotmelt Adhesive
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Thermoplastic polyurethane elastomer for soft hotmelt adhesive

Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhesive films, seam sealing tapes, heat transfer and fabric laminations, and automotive applications.

Information provided by Taiwan Sheen Soon Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 15 - 25 g/10 min
@Load 2.16 kg,
Temperature 150 °C
15 - 25 g/10 min
@Load 4.76 lb,
Temperature 302 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73 - 7773 - 77
 
Thermal PropertiesMetricEnglishComments
Softening Point 85.0 - 105 °C185 - 221 °Fflow beginning
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 10.0 - 20.0 min0.167 - 0.333 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Taiwan Sheen Soon Sheenthane® AH-580 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-650 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-620 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-592 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-591 TPU for Hotmelt Adhesive

PSHEEN825 / 156229

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.