Particle size distribution 1-250 microns. Typical distribution:- 80% < 22 microns
- 67% < 16 microns
- 43% < 10 microns
- 14% < 5 microns
Mean size is 12 microns.Master alloy blended with 3 parts iron to produce 420 alloy after sintering. SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requirements. The specifications listed are subject to the benefits and scrutiny of Osprey's accreditation to ISO 9001. Information provided to MatWeb by Osprey Metals, now Sandvik Osprey Ltd. |
UNS S42000; Powder metallurgy, MasterAlloy, Metal Powder, Metal Injection Molding, MIM, Microfine |