MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Antimonial Naval brass, UNS C46600, O61 Temper tubing
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent hot workability and hot forgeability. Fabricated by blanking, drawing, bending, heading and upsetting, hot forging, pressing.

Applications: aircraft turnbuckle barrels, balls, bolts, marine hardware, nuts, propeller shafts, rivets, valve stems, condenser plates, welding rod.

Test specimen: tubing - 9mm OD x 2.5mm wall thickness.

Inactive per the Copper Development Association.

Key Words: CDA 464, CZ133, CZ113, ISO CuZn39Sn1, CEN CW719R, UNS C46700
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 2525
Tensile Strength, Ultimate 427 MPa61900 psi
Tensile Strength, Yield 207 MPa30000 psi
Elongation at Break 45 %45 %In 50 mm, Tubing
Modulus of Elasticity 100 GPa14500 ksi
Poissons Ratio 0.280.28calculated
Fatigue Strength 100 MPa
@# of Cycles 3.00e+8
14500 psi
@# of Cycles 3.00e+8
source does not state temper
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Forgeability 90 %90 %UNS C37700 (forging brass) = 100%
Shear Modulus 39.0 GPa5660 ksi
Charpy Impact 43.0 J31.7 ft-lbkeyhole machined from plate annealed to 96 HRF
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000663 ohm-cm
@Temperature 20.0 °C
0.00000663 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.2 µm/m-°C
@Temperature 20.0 - 300 °C
11.8 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 116 W/m-K
@Temperature 20.0 °C
805 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 885 - 900 °C1630 - 1650 °F
Solidus 885 °C1630 °F
Liquidus 900 °C1650 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 650 - 825 °C1200 - 1520 °F
Recrystallization Temperature 350 °C
@Diameter 19.0 mm
662 °F
@Diameter 0.748 in
Rod cold drawn 30%
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb 0.020 - 0.10 %0.020 - 0.10 %
Copper, Cu 59 - 62 %59 - 62 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.20 %<= 0.20 %
Tin, Sn 0.50 - 1.0 %0.50 - 1.0 %
Zinc, Zn 39.25 %39.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Uninhibited Naval brass, UNS C46400, O61 Temper tubing
Arsenical Naval brass, UNS C46500, O61 Temper tubing
Phosphorized Naval brass, UNS C46700, O61 Temper tubing
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products

MC46600b1 / 11393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.