MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY GP2102 PC+GF10%
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical Resistance

Application: Mobile Phone Housing

CAS: 103598-77-2 and 65997-17-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 124124ASTM D785
Tensile Strength, Yield 54.9 MPa
@Thickness 3.20 mm
7970 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 20 %
@Thickness 3.20 mm
20 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 108 MPa
@Thickness 3.20 mm
15600 psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 3.24 GPa
@Thickness 3.20 mm
469 ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched >= 2.94 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
>= 5.51 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
@Thickness 0.750 - 0.800 mm
176 °F
@Thickness 0.0295 - 0.0315 in
UL RTI, Mechanical with Impact 80.0 °C
@Thickness 0.750 - 0.800 mm
176 °F
@Thickness 0.0295 - 0.0315 in
UL RTI, Mechanical without Impact 80.0 °C
@Thickness 0.750 - 0.800 mm
176 °F
@Thickness 0.0295 - 0.0315 in
Flammability, UL94 HB
@Thickness 0.750 - 0.800 mm
HB
@Thickness 0.0295 - 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 300 °C518 - 572 °FInjection Molding
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection Molding
Front Barrel Temperature 290 - 330 °C554 - 626 °FInjection Molding
Nozzle Temperature 290 - 330 °C554 - 626 °FInjection Molding
Melt Temperature 300 - 340 °C572 - 644 °FInjection Molding
Mold Temperature 90.0 - 120 °C194 - 248 °FInjection Molding
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPa142 - 569 psiInjection Molding
Screw Speed 40 - 70 rpm40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical HI855M PMMA, Impact Resistant Grade
LG Chemical AF342 ABS, Flame Retardant
LG Chemical LUPOL GP1000FC Flame Retardant PP
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow

PLAY527 / 148537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.