MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Xyron™ TT520 PP/PPE
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polypropylene (PP)

Material Notes: Excellent heat resistance, flame retardance, dimensional stability, and mechanical properties. Applications: Automotive parts, electrical & electronic parts, industrial parts.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccISO 1183
Filler Content 20 %20 %
Water Absorption 0.040 %
@Time 86400 sec
0.040 %
@Time 24.0 hour
Immersion; ISO 62
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in150X150X2 mm; Asahi Kasei
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psi50% RH; ISO 527
Elongation at Break 20 %20 %50%RH, nominal strain; ISO 527
Flexural Strength 64.0 MPa9280 psi50% RH; ISO 178
Flexural Modulus 3.20 GPa464 ksi50% RH; ISO 178
Charpy Impact, Notched 0.600 J/cm²
@Thickness 4.00 mm
2.86 ft-lb/in²
@Thickness 0.157 in
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.50e+16 ohm-cm5.50e+16 ohm-cm50%RH; IEC 60093
Dielectric Constant  2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
IEC 60250
 2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 41.0 kV/mm
@Thickness 2.00 mm
1040 kV/in
@Thickness 0.0787 in
short time; IEC 60243
Dissipation Factor  0.00020
@Frequency 100 Hz
0.00020
@Frequency 100 Hz
IEC 60250
 0.00070
@Frequency 1e+6 Hz
0.00070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature -30.0 - 65.0 °C
33.3 µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °FResin Temperature
Mold Temperature 50.0 - 90.0 °C122 - 194 °F
Drying Temperature 100 - 110 °C
@Time 10800 - 14400 sec
212 - 230 °F
@Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Xyron™ DG043 PPS/PPE
Asahi Kasei Xyron™ DV166 PPS/PPE
Asahi Kasei Xyron™ DG235 PPS/PPE
Asahi Kasei Xyron™ DG141 PPS/PPE
Asahi Kasei Xyron™ A0210 PA/PPE

PASAHI8249 / 221273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.