MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos ABS Lustran® ABS M406  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles.

Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm0.0060 - 0.0090 in/inTest Condition: 150x105x3; acc. ISO 2577
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm0.0060 - 0.0090 in/inTest Condition: 150x105x3; acc. ISO 2577
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 220 °C
10 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 74.0 MPa10700 psiISO 2039-1
Tensile Strength at Break 29.0 MPa4210 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 39.0 MPa5660 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 15 %>= 15 %50 mm/min; acc. ISO 527-1,-2
Elongation at Yield 2.6 %2.6 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1.80 GPa261 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 55.0 MPa7980 psi2 mm/min; ISO 178
Flexural Modulus 1.80 GPa261 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 29.0 kJ/m²
@Temperature 23.0 °C
13.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mm
@Thickness 1.00 mm
838 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0055
@Frequency 100 Hz
0.0055
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VSolution A, Rating; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2; Parallel to Flow
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C196 °FISO 75-1,-2
Vicat Softening Point 92.0 °C
@Load 5.10 kg
198 °F
@Load 11.2 lb
50°C/hour; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Glow Wire Flammability Index 650 °C1200 °FIEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FInjection Molding; ISO 294
Mold Temperature 70.0 °C158 °FInjection Molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secInjection Molding; ISO 294

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS NOVODUR® KU 2-5296 ABS, Extrusion Grade
Ineos ABS Lustran® QE 1030, Extrusion Grade
A. Schulman Diamond ABS 3500 HF Injection Molding Grade, High Flow, Medium Impact
Elix Polymers ELIX ABS P2M-AT Acrylonitrile Butadiene Styrene (ABS), High Impact Strength
A. Schulman Diamond ABS 3501ELG High Impact, Low Gloss

PINEA902 / 107173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.