MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carmel Olefins Capilene® R 50 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: CAPILENE® R 50 is a polypropylene homopolymer intended for injection molding, characterized by good flow properties combined with good balance of stiffness and impact.

APPLICATIONS

CAPILENE ® R 50 is a general purpose homopolymer. Typical applications are household articles and garden furniture.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.0 MPa4930 psiASTM D638
Elongation at Yield 11 %11 %ASTM D638
Flexural Modulus 1.55 GPa225 ksiASTM D790
Izod Impact, Notched 0.300 J/cm
@Temperature >=23.0 °C
0.562 ft-lb/in
@Temperature >=73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C207 °FASTM D648
Vicat Softening Point 155 °C
@Load 1.02 kg
311 °F
@Load 2.25 lb
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene
Braskem H 502 HC Injection Molding Polypropylene
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications
BASF Procom® D 1085 Polypropylene
BASF Novolen® 1102 K Polypropylene

PCARM024 / 79762

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.