MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyphthalamide (PPA), High Impact
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), High Impact

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.11 - 1.15 g/cc0.0401 - 0.0415 lb/in³Average value: 1.14 g/cc Grade Count:9
Water Absorption 0.500 - 0.750 %0.500 - 0.750 %Average value: 0.650 % Grade Count:4
Moisture Absorption at Equilibrium 0.700 - 2.20 %0.700 - 2.20 %Average value: 1.20 % Grade Count:3
Linear Mold Shrinkage 0.0100 - 0.0220 cm/cm0.0100 - 0.0220 in/inAverage value: 0.0169 cm/cm Grade Count:6
Linear Mold Shrinkage, Transverse 0.0100 - 0.0210 cm/cm0.0100 - 0.0210 in/inAverage value: 0.0172 cm/cm Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 55.0 - 83.4 MPa7980 - 12100 psiAverage value: 67.0 MPa Grade Count:6
 31.0 - 110 MPa
@Temperature -40.0 - 100 °C
4500 - 16000 psi
@Temperature -40.0 - 212 °F
Average value: 70.5 MPa Grade Count:2
Tensile Strength, Yield 58.0 - 80.0 MPa8410 - 11600 psiAverage value: 70.1 MPa Grade Count:6
 32.0 - 32.0 MPa
@Temperature 100 - 100 °C
4640 - 4640 psi
@Temperature 212 - 212 °F
Average value: 32.0 MPa Grade Count:1
Elongation at Break 7.00 - 80.0 %7.00 - 80.0 %Average value: 25.9 % Grade Count:9
 12.0 - 54.3 %
@Temperature -40.0 - 100 °C
12.0 - 54.3 %
@Temperature -40.0 - 212 °F
Average value: 33.2 % Grade Count:2
Elongation at Yield 5.00 - 6.00 %5.00 - 6.00 %Average value: 5.75 % Grade Count:8
 3.10 - 9.00 %
@Temperature -40.0 - 100 °C
3.10 - 9.00 %
@Temperature -40.0 - 212 °F
Average value: 6.05 % Grade Count:2
Modulus of Elasticity 1.90 - 2.76 GPa276 - 400 ksiAverage value: 2.41 GPa Grade Count:9
 1.80 - 2.00 GPa
@Temperature 100 - 100 °C
261 - 290 ksi
@Temperature 212 - 212 °F
Average value: 1.90 GPa Grade Count:2
Flexural Yield Strength 66.0 - 128 MPa9570 - 18600 psiAverage value: 100 MPa Grade Count:7
 42.0 - 49.6 MPa
@Temperature 100 - 100 °C
6090 - 7190 psi
@Temperature 212 - 212 °F
Average value: 45.2 MPa Grade Count:3
Flexural Modulus 1.79 - 2.60 GPa260 - 377 ksiAverage value: 2.29 GPa Grade Count:8
 1.30 - 1.72 GPa
@Temperature 100 - 100 °C
189 - 249 ksi
@Temperature 212 - 212 °F
Average value: 1.44 GPa Grade Count:3
Poissons Ratio 0.350 - 0.3900.350 - 0.390Average value: 0.360 Grade Count:4
Shear Strength 53.0 - 64.1 MPa7690 - 9300 psiAverage value: 58.6 MPa Grade Count:3
Izod Impact, Notched 1.10 - 11.0 J/cm2.06 - 20.6 ft-lb/inAverage value: 7.41 J/cm Grade Count:7
 7.50 - 7.50 J/cm
@Temperature -40.0 - -40.0 °C
14.1 - 14.1 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 7.50 J/cm Grade Count:1
Izod Impact, Notched (ISO) 13.0 - 80.0 kJ/m²6.19 - 38.1 ft-lb/in²Average value: 46.5 kJ/m² Grade Count:4
 18.0 - 18.0 kJ/m²
@Temperature -30.0 - -30.0 °C
8.57 - 8.57 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 18.0 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) NBNBGrade Count:3
Charpy Impact Unnotched 1000 J/cm² - NB4760 ft-lb/in² - NBGrade Count:4
 999.9 - 999.9 J/cm²
@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Grade Count:1
Charpy Impact, Notched 1.30 J/cm² - NB6.19 ft-lb/in² - NBAverage value: 5.70 J/cm² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 - 1.20e+16 ohm-cm1.00e+15 - 1.20e+16 ohm-cmAverage value: 4.67e+15 ohm-cm Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 - 140 µm/m-°C
@Temperature 100 - 200 °C
72.2 - 77.8 µin/in-°F
@Temperature 212 - 392 °F
Average value: 135 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 110 - 140 µm/m-°C
@Temperature 100 - 200 °C
61.1 - 77.8 µin/in-°F
@Temperature 212 - 392 °F
Average value: 125 µm/m-°C Grade Count:2
Specific Heat Capacity 2.90 - 2.90 J/g-°C
@Temperature 325 - 325 °C
0.693 - 0.693 BTU/lb-°F
@Temperature 617 - 617 °F
Average value: 2.90 J/g-°C Grade Count:1
Melting Point 300 - 315 °C572 - 599 °FAverage value: 310 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 109 - 125 °C228 - 257 °FAverage value: 118 °C Grade Count:7
Flammability, UL94 HBHBGrade Count:3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 304 - 343 °C579 - 649 °FAverage value: 323 °C Grade Count:6
Mold Temperature 70.0 - 135 °C158 - 275 °FAverage value: 113 °C Grade Count:4
Drying Temperature 100 - 120 °C212 - 248 °FAverage value: 110 °C Grade Count:5
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.0870 % Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA)
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
RTP Company RTP 4087 Polyphthalamide (PPA); Carbon Fiber

O4602 / 78358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.