During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micro-organisms, such as algae, bacteria and fungi. The antimicrobial effect remains during the entire life time of the product. POM CG-plastics are often used in medical and food products and facilities due additional protection.Information provided by CENTROPLAST Engineering Plastics GMBH |