MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lanxess Bayscript® Yellow 4GF Pigment
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes:

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 g/cc0.0145 lb/in³DIN ISO 787-11
Density 1.80 g/cc0.0650 lb/in³DIN ISO 787-10
Water Absorption 3.0 %3.0 %
Particle Size <= 0.20 µm<= 0.20 µmX99
pH 5.0 - 7.05.0 - 7.0DIN ISO 9277
Specific Surface Area 110 m²/g110 m²/gDIN ISO 9277
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 5000 ohm-cm>= 5000 ohm-cm
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month60.0 Month
 
Descriptive Properties
AppearanceYellow with a green cast powder
Specifications1/25 STLight fastness
 1/3 STLight fastness
 200°CHeat Stability

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMCAL ENSACO™ 260G Conductive Carbon Black
Lanxess Rhenosin® W 759 Rubber Plasticizer
BASF Theroplast® Black X70 Color Additive
BASF Paliogen® Red L 3910 HD Color Additive

PLANY8452 / 208845

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.