MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman BMC 324 Automotive Grade Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-coat. BMC 324 can be supplied in logs, slugs or bulk form.

Typical applications include Automotive Headlamp and Foglamp Reflectors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 2.00 g/cc1.80 - 2.00 g/cc
Water Absorption 0.10 - 0.30 %0.10 - 0.30 %24 hours, 23°C
Linear Mold Shrinkage 0.00 - 0.0020 cm/cm0.00 - 0.0020 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 40 - 6040 - 60
Tensile Strength, Ultimate 27.6 - 55.2 MPa4000 - 8000 psi
Flexural Strength 82.7 - 124 MPa12000 - 18000 psi
Flexural Modulus 7.58 - 13.1 GPa1100 - 1900 ksi
Compressive Strength 110 - 138 MPa16000 - 20000 psi
Izod Impact, Notched 1.07 - 3.74 J/cm2.00 - 7.00 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C425 - 500 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Mold Temperature 171 - 193 °C340 - 380 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC 304 Automotive Grade Molding Compound
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman BMC 100 Thermoset Polyester, GP
A. Schulman BMC 300 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer

PBMC006 / 27189

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.