MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Appryl® CZU 0525 Polypropylene, 25% Talc Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for exterior trim automotive applications, that required an excellent impact test associated with a high modulus.

It is UV stabilized and has a good paintability.

Main application is side panels.

ISO data provided by the manufacturer, Arkema.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.0 MPa2760 psi50 mm/min
Elongation at Break 26 %26 %Nominal Strain; 50 mm/min
Elongation at Yield 4.0 %4.0 %50 mm/min
Tensile Modulus 1.92 GPa278 ksi1 mm/min
Charpy Impact Unnotched NBNB
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²
 0.360 J/cm²
@Temperature -30.0 °C
1.71 ft-lb/in²
@Temperature -22.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 161 °C322 °F10°C/min
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °F
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °F
Vicat Softening Point 52.0 °C126 °F50°C/hr; 50N

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® C30 TR/25 25% Talc Reinforced Polypropylene Copolymer
Overview of materials for Polypropylene with 10% Talc Filler
Overview of materials for Polypropylene with 30% Talc Filler
Arkema Appryl® CZN 0525 Polypropylene, 25% Talc Filled
Overview of materials for Polypropylene with 20% Talc Filler

PZARKG222 / 25513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.