MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Kalrez® AeroSeal™ 7777 Fluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DuPont™ Kalrez AeroSeal™ 7777 perfluoroelastomer parts are a specialty black product that meets the requirements of Aerospace Material Specification (AMS) 7257C. It offers outstanding thermal stability and compression set resistance along with excellent seal force retention properties. It also offers excellent resistance to HTS (High Thermo-Oxidative Stability) gas turbine engine lubricating oils and has excellent response to temperature cycling effects. Kalrez AeroSeal™ 7777 has good mechanical properties and is well suited for both static and dynamic sealing applications. A maximum continuous service temperature of 325 C (617 F) is suggested. Short excursions to higher temperatures may also be possible.

Performance Features/Benefits

  • Outstanding thermal stability
  • Outstanding compression set resistance
  • Excellent seal force retention properties
  • Excellent resistance to high thermo-oxidative stability (HTS) gas turbine engine lubricating oils
  • Excellent response to temperature cycling effects
  • Excellent mechanical properties
  • Lower coefficient of thermal expansion (CTE) versus other Kalrez® products thus minimizing the need to increase the free volume of the seal gland when upgrading from fluoroelastomers (FKM) to perfluoroelastomers (FFKM) to Kalrez® AeroSeal™ 7777.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575ASTM D2240
Tensile Strength at Break 17.91 MPa2598 psiASTM D412
Elongation at Break 160 %160 %ASTM D412
100% Modulus 7.58 MPa
@Strain 100 %
1100 psi
@Strain 100 %
ASTM D412
Compression Set  15 %
@Temperature 204 °C,
Time 252000 sec
15 %
@Temperature 399 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
 19 %
@Temperature 300 °C,
Time 252000 sec
19 %
@Temperature 572 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
 34 %
@Temperature 325 °C,
Time 252000 sec
34 %
@Temperature 617 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 325 °C617 °FDuPont Test Method
Minimum Service Temperature, Air -4.00 °C24.8 °FRetraction Temperature, Tr10; ASTM D1329
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® AeroSeal™ 7797 Fluoroelastomer
Chemours Viton® A-HV Fluoroelastomer (FKM)
Colorite Polymers 7777 Non-Phthalate 77 Series Vinyl Compound
DuPont Mobility and Materials Kalrez® 1045 Fluoroelastomer

PDVC9779 / 170420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.