MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Diamond SAN 330 BEADS Styrene Acrylonitrile, Transparent Engineering Thermoplastic, High Flow Natural Beads
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Styrene Acrylonitrile
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow  8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 31.1 g/10 min
@Load 3.80 kg,
Temperature 230 °C
31.1 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 68.9 MPa9990 psichs 2.0 in/min; ASTM D638
Flexural Modulus 3.445 GPa499.7 ksichs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 0.214 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
0.401 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C
@Load 1.00 kg,
Thickness 3.17 mm
212 °F
@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond SAN 267 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Entec Hyril® GP355AS Styrene Acrylonitrile
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
Avient Edgetek® PF-20GF/000 Polysulfone (PSU)
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon

PDIAM488 / 126579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.