MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Reltek SEALiT™ A-46 Clear Coat & Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties:
  • Optical clear coat for metals, glass and ceramic.
  • Sealant for ceramic, electronic components (e.g. flex-PCB’s exposed to moisture).
  • Architectural coating.

Applications: Handles continuous temperatures to 250°C (500°F). Excellent moisture seal and exterior environment protection. Maintains clear coat under UV exposure to sunlight. Seals micro-pores. Wets siliceous substrates easily, self leveling to 2 mil coating, pinhole free in one coat. Good coating for stainless steel, copper and aluminum architectural coating. Ambient cure 60 min or accelerated thermal cure.

Key Words: Epoxy Adhesive, Sealant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.018 - 1.038 g/cc1.018 - 1.038 g/ccASTM D1298
Viscosity Measurement 4.5 - 8.54.5 - 8.5ASTM D445
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.442 - 1.4481.442 - 1.448ASTM D1218
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourAmbient
 5.00 min
@Temperature 150 °C
0.0833 hour
@Temperature 302 °F
 15.0 min
@Temperature 75.0 °C
0.250 hour
@Temperature 167 °F
 
Descriptive Properties
ColorClear with stray color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Zirconia ZYF-150 Zirconia Felt Insulation
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
NRI Syntho-Shield™

PAQREL12 / 24228

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.