MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

C.O.I.M. LARIPUR® LPR6560 PTMG Polyether Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 60 and E 2103 PTMG Ether: These products are based on PTMG polyether. In comparison to the LARIPUR® ester series, they show a higher resistance to hydrolysis and microbiological attacks, have higher cold flexibility but have lower thermal and oxidizing resistance.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 67.4 MPa9780 psiASTM D412
Elongation at Break 340 %340 %ASTM D412
50% Modulus 22.2 MPa
@Strain 50 %
22.2 MPa
@Strain 50 %
ASTM D412
100% Modulus 26.3 MPa
@Strain 100 %
3810 psi
@Strain 100 %
ASTM D412
300% Modulus 50.5 MPa
@Strain 300 %
7320 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.400 GPa58.0 ksiASTM D790
Izod Impact, Notched (ISO) 8.10 kJ/m²
@Temperature -20.0 °C
3.85 ft-lb/in²
@Temperature -4.00 °F
ASTM D256
Tear Strength 175 kN/m999 pliASTM D624
Abrasion 3535mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 87.0 MPa12600 psi+20°C; ASTM D1043
 330 MPa47900 psi-20°C; ASTM D1043
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 138 °C280 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR6260 PTMG Polyether Polyurethane
BASF Elastollan® 1154 D KFFC TPUR
C.O.I.M. LARIPUR® LPR5760 PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR6520 Standard Adipate Ester Polyurethane

PCOIM032 / 28635

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.