MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 6101-H111
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A96101; ISO E-AlMgSi; Aluminium 6101-H111; AA6101-H111; Al6101-H111
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.70 g/cc0.0975 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 2626500 kg load with 10 mm ball. Calculated value.
Tensile Strength, Ultimate 96.5 MPa14000 psiAA; Typical
Tensile Strength, Yield 75.8 MPa11000 psiAA; Typical
Modulus of Elasticity 69.0 GPa10000 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 60.0 MPa8700 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000280 ohm-cm0.00000280 ohm-cmEstimated from other heat treatments.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.7 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.1 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
 24.4 µm/m-°C
@Temperature 20.0 - 200 °C
13.6 µin/in-°F
@Temperature 68.0 - 392 °F
 25.4 µm/m-°C
@Temperature 20.0 - 300 °C
14.1 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.895 J/g-°C0.214 BTU/lb-°F
Thermal Conductivity 220 W/m-K1530 BTU-in/hr-ft²-°FEstimated from other heat treatments.
Melting Point 620 - 655 °C1150 - 1210 °F
Solidus 620 °C1150 °F
Liquidus 655 °C1210 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 510 °C950 °Fhold at temperature for 1 hr
Aging Temperature 177 °C350 °Fhold at temperature for 6 to 8 hr
Hot-Working Temperature 260 - 510 °C500 - 950 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 97.6 %<= 97.6 %As remainder
Boron, B <= 0.06 %<= 0.06 %
Chromium, Cr <= 0.03 %<= 0.03 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.50 %<= 0.50 %
Magnesium, Mg 0.35 - 0.80 %0.35 - 0.80 %
Manganese, Mn <= 0.03 %<= 0.03 %
Other, each <= 0.03 %<= 0.03 %
Other, total <= 0.10 %<= 0.10 %
Silicon, Si 0.30 - 0.70 %0.30 - 0.70 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6101-T6
Aluminum 6101-T65
Aluminum 6101-T61
Aluminum 6101-T63
Aluminum 6101-T64

MA6101H111 / 9441

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.