MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGO® AddBond DS 1300 Adhesion resin solution
Categories: Other Engineering Material

Material Notes: Special features:
  • for waterborne formulations
  • excellent adhesion improvement on aluminum, steel and galvanized steel as well as on plastics, e.g. PVC and ABS
  • improves the intercoat adhesion
  • improves the corrosion protection
  • improves flexibility
  • improves the gloss
  • free of organic solvents
Application:
  • Industrial coatings recommended addition level solid calculated on binder solid: 2.5 - 10.0 %

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 55 %55 %
pH 7.07.0
Viscosity 100 cP100 cP
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 30.0 °C86.0 °Fsolid resin
 
Descriptive Properties
Hydroxyl Number60 mg KOH/gcalculated on non-volatile content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGO® AddBond LTH Solid adhesion resin
Evonik TEGO® AddBond 2220 ND Adhesion resin solution
Evonik TEGO® AddBond 2325 Adhesion resin solution
Dow P5204 ADHESION PROMOTER
Evonik TEGO® AddBond 1270 Adhesion resin solution

PEVONIL667 / 196871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.