MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis HD204CF Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extrusion, blending, textile packaging film, food packaging, lamination films, stationery folders, manufacturing of unoriented film for producers who wish to add their own slip/antiblock/antistatic additive package, and blending with formulated grades for additive adjustments. HD204CF free of slip and antiblock and without CaStearate.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.910 g/cc0.0325 - 0.0329 lb/in³base resin; ISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 - 700 %500 - 700 %ISO 527-3
Film Elongation at Break, TD 500 - 700 %500 - 700 %ISO 527-3
Tensile Modulus 0.650 - 0.750 GPa94.3 - 109 ksiISO 527-3
Flexural Modulus 1.35 GPa196 ksi5mm/min; ISO 178
Puncture Energy 14.0 J10.3 ft-lb1100N; ISO 7765-2
Coefficient of Friction >= 0.70>= 0.70film to film; ISO 8295
Film Tensile Strength at Break, MD 30.0 - 50.0 MPa4350 - 7250 psiISO 527-3
Film Tensile Strength at Break, TD 25.0 - 45.0 MPa3630 - 6530 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 162 - 166 °C324 - 331 °FDSC; ISO 3146
Vicat Softening Point 152 °C
@Load 5.10 kg
306 °F
@Load 11.2 lb
A50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 2.0 %<= 2.0 %ASTM D1003
Gloss >= 120 %>= 120 %20° of arc; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HD234CF Polypropylene
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Borealis HD120MO Polypropylene
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)

PBOREA474 / 108733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.