MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupox® PBT-GP-1000 High Flow PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ASTM D792
Water Absorption 0.080 %0.080 %24 hours at 73°F; ASTM D570
Linear Mold Shrinkage 0.012 - 0.021 cm/cm0.012 - 0.021 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength, Ultimate 56.5 MPa
@Thickness 3.17 mm
8190 psi
@Thickness 0.125 in
ASTM D638
Tensile Strength, Yield 53.8 MPa7800 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Flexural Yield Strength 83.4 MPa12100 psiASTM D570
Flexural Modulus 2.25 GPa327 ksiASTM D570
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 130 sec130 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 0.7937 mm
HB
@Thickness 0.03125 in
UL94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 225 - 235 °C437 - 455 °F
Middle Barrel Temperature 230 - 240 °C446 - 464 °F
Front Barrel Temperature 235 - 245 °C455 - 473 °F
Nozzle Temperature 235 - 249 °C455 - 480 °F
Melt Temperature 235 - 249 °C455 - 480 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °FSurface
Drying Temperature 120 °C248 °F5 hr.
 140 °C284 °F3 hr.
 120 °C
@Time 18000 sec
248 °F
@Time 5.00 hour
 140 °C
@Time 10800 sec
284 °F
@Time 3.00 hour
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Shot Size 30 - 80 %30 - 80 %
Vent Depth 0.00254 - 0.00381 cm0.00100 - 0.00150 in
 
Descriptive Properties
Ram Speed SettingMedium to Fast
Screw SpeedSlow to Medium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupox® GP1000D PBT
LG Chemical LUPOY GP-1000 General Purpose Modified PC, Unreinforced
LG Chemical Lupox® TE5006F PET+PC
LG Chemical Lupox® TE5000D PBT+PC
LG Chemical Lupox® GP1006FD PBT

PLBA02 / 50359

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.