MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NuSil MED-340 Simethicone USP/EP
Categories: Polymer; Thermoset; Silicone

Material Notes: NuSil’s MED-342 is a 30% simethicone granular solid. This product is produced using a patented process that applies the simethicone to maltodextrin without the use of solvents. The simethicone used in the formulation meets the USP monograph for simethicone and the EP monograph for simeticonum. It is the fastest granular simethicone defoamer on the market and a proven history of use in chewable and soft chew tablets currently on the market.
  • A unique solid that allows for easy blending with other tablet ingredients
  • Reduces cost of clean-up and additional equipment required for liquid addition of Simethicone active
  • Fully assayed for simethicone content and uniformity. The assay of each lot is provided on the Certificate of Analysis to allow formulators to easily calculate the amount of granular simethicone required for specific products.
  • Contains all Compendial grade components suitable for oral use
  • Can be combined with flavors and lubricants
Applications:
  • For the manufacture of single- or double-layer tablets
  • For forming uniform compositions in any concentration required
  • For effective, stable antiflatulence, even in the presence of aluminum and magnesium hydroxide

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1600 cP1600 cP
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
ColorTranslucent gray liquid
Composition<5 ppmHeavy Metals
 0.95PDMS Content
 1Simethicone Content
Defoaming Test3 sec
Loss on Heating0.0025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecophilic® TG-500 Hydrophilic TPU Hydrogel
Shin-Etsu Silicones KSG-15 Fluid
Aluminum, Al
Borosilicate Glass
BASF Ecoflex® C1200 F Blend Biodegradable Polyester

PNUSIL482 / 142206

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.