MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well suited for consumer goods and industrial applications requiring non-slip/soft dry-touch ergonomics, sound and vibration dampening, improved impact resistance, and U.V. stability. Elastocon® STK40B can be overmolded to PC, ABS, PC/ABS, Acrylic, HIPS, copolyester, various grades of polyamide, and more.

Information provided by Elastocon TPE Technologies, Inc. Elastocon® TPE Technologies has been acquired by Aurora Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm0.015 - 0.025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM D2240
Tensile Strength 2.96 MPa429 psiASTM D412
Elongation at Break 338 %338 %ASTM D412
100% Modulus 1.38 MPa
@Strain 100 %
200 psi
@Strain 100 %
ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 216 °C410 - 420 °F
Front Barrel Temperature 216 - 266 °C420 - 510 °F
Nozzle Temperature 227 - 277 °C440 - 530 °F
Mold Temperature 26.7 - 48.9 °C80.0 - 120 °F
Injection Velocity 25.4 - 127 mm/sec1.00 - 5.00 in/sec
Back Pressure 0.517 - 1.21 MPa75.0 - 175 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 500400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Translucent
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer
Avient OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE)

PELASC309 / 142485

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.