MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Top Polymer Topolymer® 6200-T/C/A TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Production Description: Topolymer® 6200-T/C/A is a transparent compound which made from SBS (styrene isoprene/butadiene block copolymer), It was designed specially for toys that need painting.

Features: High transparency, Paintable, High gloss, Excellent tear resistant and flexibility

Information provided by Top Polymer Enterprise

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 - 0.920 g/cc0.890 - 0.920 g/cc
Linear Mold Shrinkage 0.018 - 0.025 cm/cm0.018 - 0.025 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5.0 - 855.0 - 85
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 130 - 150 °C266 - 302 °FInjection
Middle Barrel Temperature 170 - 190 °C338 - 374 °FInjection
Front Barrel Temperature 170 - 200 °C338 - 392 °FInjection
Nozzle Temperature 170 - 200 °C338 - 392 °FInjection
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection
Injection Pressure 3.00 - 10.0 MPa435 - 1450 psiInjection
Screw Speed 30 - 80 rpm30 - 80 rpmInjection
 
Descriptive Properties
ColorTransparent, glossy
Screw L/D22:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Top Polymer Topolymer® 8209-P TPE
Top Polymer Topolymer® 6211-N TPE
Polymax® Maxelast® C4902 TPE, Transparent
STAR Thermoplastic Alloys & Rubbers Starflex® P 7007 Thermoplastic Elastomer
Stellarchem MP-8001 TPE Compound

PTOPO029 / 184541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.