MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Microthene MP652962 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Microthene MP652962 is a hexene HDPE powder selected for rotationally molding large tank applications. MP652962 is a UV-stabilized, 35-mesh powder and is also available in pellet form as Petrothene GA652962. Applications: Containers, Intermediate Bulk Containers, Tanks, Industrial.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³ASTM D1505
ESCR 100% Igepal® >= 400 hour>= 400 hourCond. A; ASTM D1693
ESCR 10% Igepal® >= 50 hour>= 50 hourCond. A; ASTM D1693
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.4 MPa3390 psiASTM D638
Flexural Modulus, 1% Secant 1010 MPa146000 psiASTM D790
2% Secant Modulus 0.855 GPa124 ksiASTM D790
Impact Test  55.0 J
@Temperature -40.0 °C
40.6 ft-lb
@Temperature -40.0 °F
1/4" specimen, ARM
 215 J
@Temperature -40.0 °C
159 ft-lb
@Temperature -40.0 °F
1/4" specimen, ARM
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C149 °Funannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C109 °Funannealed; ASTM D648
 
Descriptive Properties
Processing MethodRotomolding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LLP8460.29 Rotational Molding Resin
Braskem RC35U4 LLDPE Rotomolding Polyethylene
Braskem ML4400N LLDPE Rotomolding Polyethylene
LyondellBasell Petrothene GA652962 High Density Polyethylene (HDPE), Rotational Molding Grade
LyondellBasell Petrothene PM96750

PEQT7616 / 219253

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.