MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnForce™ LFT NN-50LGF/000 HS UV Black Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. These products exhibit enhanced physical and mechanical properties versus standard short fiber products. Benefits of LFT compounds include improved impact strength, elastic modulus, and material strength across wide temperature ranges from subambient to highly elevated. Furthermore, LFT compounds have been shown to offer improved performance in the areas of creep and fatigue performance, improved dimensional stability, and exhibit an exceptional surface finish when compared to traditional highly filled short fiber products.

LFT compounds can be processed using equipment similar to that used for short fiber products. The mechanical properties of finished parts depend greatly on the length of the fibers in the molded part; therefore processing conditions must be set carefully in order to minimize fiber breakage. A low shear process is advised, with low back pressure, low screw speed and low-to-medium injection speed.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ISO 1183
Filler Content 50 %50 %Long Glass Fiber
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inMeasured on a tensile specimen.; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 230 MPa33400 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 14.5 GPa2100 ksiISO 527-2
Flexural Strength 330 MPa47900 psiISO 178
Flexural Modulus 13.0 GPa1890 ksiISO 178
Charpy Impact Unnotched 7.50 J/cm²35.7 ft-lb/in²ISO 179
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179
Gardner Impact 12.7 J9.37 ft-lbASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 252 °C486 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 235 °C455 °FUnannealed; ISO 75-2/C
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 320 °C554 - 608 °F
Mold Temperature 90.0 °C194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour
Back Pressure 1.00 MPa145 psi
 
Descriptive Properties
FeaturesGood UV Resistance
 Heat Stabilized
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Injection RateSlow-Moderate
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnForce™ LFT NN-50LGF/000 HS Black Polyamide 66 (Nylon 66)
RTP Company RTP 2099 X 134514 Polycarbonate/Polyester Flame Retardant - UV Stabilized - Chemical Resistant Alloy
RTP Company RTP 2099 X 137399 A NS Polyester Alloy Flame Retardant - UV Stabilized - Medical Cleaner Resistant - No Subs
RTP Company RTP 203A UV  Nylon 6 (PA 6) Glass Fiber 20% - UV Stable

PH0POL1382 / 145951

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.