MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Ateva® 1231 Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Ateva® 1231 resin is designed for medical and other tubing applications, it is also well suited for high quality microcellular crosslinked foam applications. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives:

Applications: Foam; Medical; Tubes & Pipes

Information provided by Celanese Corporation.

Key Words: medical and other tubing applications; high quality microcellular crosslinked foam
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.934 g/cc0.0337 lb/in³ASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 12 %12 %AT Plastics PTM-39
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Hardness, Shore D 4242ASTM D2240
Tensile Strength at Break 16.0 MPa2320 psiType IV (50 mm/min); ASTM D638
Elongation at Break 730 %730 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 82.0 MPa11900 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.0 °C207 °FDSC; ASTM D3417
Vicat Softening Point 75.0 °C167 °FASTM D1525
Brittleness Temperature <= -85.0 °C<= -121 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 1030 Ethylene Vinyl Acetate Copolymer
Celanese Ateva® 1081 Ethylene Vinyl Acetate Copolymer
Covestro Desmopan® W DP89043D Polyurethane
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer
Celanese Ateva® 1030 Film Ethylene Vinyl Acetate Copolymer Film

PATEVB49 / 26005

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.