MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Rulon® 1045 Bearing/Seal PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Rulon® 1045 is a dull gold material that has an excellent ability to elongate in a flip seal application. Coupled with excellent frictional characteristics, it offers the added benefit of energy savings, as well as increased sealing efficiency.

This material is also resistant to many harsh chemicals found in the application environments where it is typically used. It is also compatible with most commercially available lubricants for additional reduction in friction. Its low deformation properties allow it to be effective as a bearing or sliding surface.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.11 g/cc0.0762 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 26.9 MPa3900 psiASTM D638
Elongation at Break 450 %450 %ASTM D638
Compressive Yield Strength 6.89 MPa1000 psiMax load under tribological use
Coefficient of Friction, Dynamic 0.10 - 0.200.10 - 0.20Dry vs. Steel
Coefficient of Friction, Static 0.10 - 0.200.10 - 0.20Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec9990 psi-ft/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 117 µm/m-°C
@Temperature 25.6 - 93.3 °C
65.0 µin/in-°F
@Temperature 78.0 - 200 °F
Length
CTE, linear, Transverse to Flow 117 µm/m-°C
@Temperature 25.6 - 93.3 °C
65.0 µin/in-°F
@Temperature 78.0 - 200 °F
Diameter
 
Descriptive Properties
Application EnvironmentDry
 Vacuum
 Wet
ColorDull Gold

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polikim EFALON® T-100 Virgin PTFE
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE
Saint-Gobain Rulon® LR Bearing/Seal PTFE
Adamas Adalon® 992 Modified PTFE
Saint-Gobain Rulon® J Bearing/Seal PTFE

PSTGQ990 / 108547

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.