MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 08112 Polyester BMC, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its combination of high heat resistance, good electrical properties and strength, it can be used in such applications as iron skirts and other small appliance housings, coil bobbins, and electric motor components such as brush holders. It is available in either bulk or extruded form and is currently available in natural. Other colors are available upon request. It is UL recognized under file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.03 g/cc0.0733 lb/in³ASTM D792
Water Absorption 0.093 %0.093 %ASTM D570
Linear Mold Shrinkage 0.00228 cm/cm0.00228 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 5252ASTM D785
Tensile Strength, Ultimate 39.0 MPa5660 psiASTM D638
Elongation at Break 0.39 %0.39 %ASTM D638
Tensile Modulus 16.6 GPa2410 ksiASTM D638
Flexural Strength 89.0 MPa12900 psiASTM D790
Flexural Modulus 14.0 GPa2030 ksiASTM D790
Compressive Strength 125 MPa18100 psiASTM D695
Izod Impact, Notched 2.37 J/cm4.44 ft-lb/inASTM D256
Charpy Impact, Notched 2.31 J/cm²11.0 ft-lb/in²ASTM D256
Impact 810810J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.90e+15 ohm-cm9.90e+15 ohm-cmASTM D247
Dielectric Constant 4.94.9ASTM D150
Dielectric Strength 9.70 kV/mm246 kV/inStep by Step; ASTM D149
 11.8 kV/mm300 kV/inShort Time; ASTM D149
Dielectric Breakdown 23000 V23000 V1hr 120C; ASTM D149
Dissipation Factor 0.00960.0096ASTM D150
Arc Resistance 188 sec188 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 228 °C442 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 267 °C513 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Shrinkage 0.00 %0.00 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IDI Composites Rosite® 3950D BMC Thermoset Polyester, 25% Glass Reinforced
IDI Composites Dielectrite® 48-50 Thermoset Polyester, Molding
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound

PLEM55m0 / 50738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.