MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Cellulose Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 - 1.57 g/cc0.0556 - 0.0567 lb/in³Average value: 1.56 g/cc Grade Count:5
Water Absorption 0.163 - 0.224 %0.163 - 0.224 %Average value: 0.201 % Grade Count:5
Linear Mold Shrinkage 0.00283 - 0.00760 cm/cm0.00283 - 0.00760 in/inAverage value: 0.00493 cm/cm Grade Count:5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 77.0 - 84.077.0 - 84.0Average value: 80.2 Grade Count:5
Tensile Strength, Ultimate 44.0 - 55.0 MPa6380 - 7980 psiAverage value: 50.6 MPa Grade Count:5
Elongation at Break 0.440 - 0.700 %0.440 - 0.700 %Average value: 0.596 % Grade Count:5
Modulus of Elasticity 9.90 - 11.3 GPa1440 - 1640 ksiAverage value: 10.4 GPa Grade Count:5
Flexural Yield Strength 74.0 - 92.0 MPa10700 - 13300 psiAverage value: 81.2 MPa Grade Count:5
Flexural Modulus 8.60 - 10.5 GPa1250 - 1520 ksiAverage value: 9.44 GPa Grade Count:5
Compressive Yield Strength 162 - 195 MPa23500 - 28300 psiAverage value: 177 MPa Grade Count:5
Izod Impact, Notched 0.160 - 0.202 J/cm0.300 - 0.378 ft-lb/inAverage value: 0.175 J/cm Grade Count:5
Charpy Impact, Notched 0.168 - 0.215 J/cm²0.800 - 1.02 ft-lb/in²Average value: 0.195 J/cm² Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.00e+11 - 3.00e+12 ohm-cm3.00e+11 - 3.00e+12 ohm-cmAverage value: 1.39e+12 ohm-cm Grade Count:5
Dielectric Constant 5.10 - 5.705.10 - 5.70Average value: 5.40 Grade Count:5
Dielectric Strength 6.60 - 14.9 kV/mm168 - 378 kV/inAverage value: 11.3 kV/mm Grade Count:5
Dissipation Factor 0.0380 - 0.07400.0380 - 0.0740Average value: 0.0542 Grade Count:5
Arc Resistance 171 - 182 sec171 - 182 secAverage value: 178 sec Grade Count:5
Comparative Tracking Index 175 - 200 V175 - 200 VAverage value: 180 V Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.0 - 52.0 µm/m-°C
@Temperature 40.0 - 130 °C
25.6 - 28.9 µin/in-°F
@Temperature 104 - 266 °F
Average value: 48.0 µm/m-°C Grade Count:3
Thermal Conductivity 0.540 - 0.540 W/m-K
@Temperature 100 - 100 °C
3.75 - 3.75 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 0.540 W/m-K Grade Count:2
Maximum Service Temperature, Air 196 - 203 °C385 - 397 °FAverage value: 201 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 173 - 197 °C343 - 387 °FAverage value: 187 °C Grade Count:5
Flammability, UL94 V-0V-0Grade Count:5
Oxygen Index 28.0 - 33.0 %28.0 - 33.0 %Average value: 30.7 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
Overview of materials for Phenolic, Novolac, Cellulose Filled
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate
Bakelite® PF 31 Phenolic Formaldehyde Resin, UL Listed

O2721 / 78091

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.