MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer
Categories: Polymer; Film; Thermoplastic

Material Notes: Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The material also is recommended for contour extrusion, as well as for blow molding of toys, gaskets and other parts requiring flexibility, stress cracking resistance and low temperature toughness. Elvaloy® 2112 AC also can be used in film applications where softness and flexibility are needed.

Elvaloy® 2112 AC has a wide processing latitude in molding and extrusion equipment. EEA is very heat stable and does not give corrosive decomposition products during processing, even at the upper limit of the recommended temperature range.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792 - ISO 1183
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240 - ISO 868
Hardness, Shore D 3535ASTM D2240 - ISO 868
Tensile Strength at Break 16.0 MPa2320 psi500 mm/min; ASTM D638 - ISO 527-2
Elongation at Break 700 %700 %500 mm/min; ASTM D638 - ISO 527-2
Tensile Modulus 0.0570 GPa8.27 ksi1 mm/min; ASTM D638 - ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 99.0 °C210 °FBy DSC; ASTM D3418 - ISO 3146
Vicat Softening Point 69.0 °C156 °FA50 (10N); ASTM D1525 - ISO 306
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 150 °C302 °FExtrusion lamination and extrusion coating
 150 °C302 °FCast film
 150 °C302 °FBlown film
Middle Barrel Temperature 160 °C320 °FBlown film
 210 °C410 °FCast film
 220 °C428 °FExtrusion lamination
Front Barrel Temperature 170 °C338 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
Adapter Temperature 180 °C356 °FBlown film
 250 °C482 °FCast Film
 290 °C554 °FExtrusion lamination
Die Temperature 180 °C356 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
Melt Temperature 160 - 220 °C320 - 428 °FFor blow molding
 
Descriptive Properties
EA-Content12 wt.%DuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Dow Elvaloy® HP662 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer

PDUPM059 / 33726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.