MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Wacker Silpuran® 6700/40 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product description: Liquid silicone rubber of the SILPURAN® 6700 series is a paste-like, easily-pigmentable two-component compound with a very short curing time and good mechanical and electrical properties. Vulcanizates are noted for their self-adhesive properties to various substrates.

Properties: SILPURAN® 6700/40 A/B meets selected test requirements of ISO 10993 and United States Pharmacopoeia (USP) Class VI. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Special features: SILPURAN® 6700/40 A/B is a primerless selfbonding grade that adheres to various thermoplasts (e.g. PA, PBT) and metals. The bonding is improved by an ageing process (e.g. one hour at 100 °C) or by a longer storage at room temperature. Because of the individual surface properties each substrate must be tested before mass production. If necessary one has to check the development of adhesive properties over time and/or in an environment relevant to the application.

Application: SILPURAN® 6700/40 A/B is particularly suitable for the economical production of large series of injection-moulded articles. SILPURAN® 6700/40 A/B is designed for medical and pharmaceutical applications including implantation for < 30 days.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³DIN EN ISO 1183-1 A
Viscosity  260000 cP
@Shear Rate 10.0 1/s
260000 cP
@Shear Rate 10.0 1/s
DIN 53019
 760000 cP
@Shear Rate 1.00 1/s
760000 cP
@Shear Rate 1.00 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040DIN 53505
Tensile Strength at Break 7.70 MPa1120 psiDIN 53505 S1
Elongation at Break 610 %610 %DIN 53505 S1
Rebound 60 %60 %DIN 53512
Tear Strength 23.0 kN/m131 pliASTM D624B
Compression Set  40 %
@Temperature 125 °C,
Time 79200 sec
40 %
@Temperature 257 °F,
Time 22.0 hour
DIN ISO 815-B
 55 %
@Temperature 150 °C,
Time 79200 sec
55 %
@Temperature 302 °F,
Time 22.0 hour
DIN ISO 815-B
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Colortransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3003/03 A/B Liquid Silicone Rubber
Celanese Celanex® 2402 MT PBT, Medical Technology
Celanese Celanex® 2401 MT PBT, Medical Technology
Celanese Celanex® 2404 MT PBT, Medical Technology

PWACK9503 / 205032

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.