MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Keltan® 9950C Ethylene-Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Amorphous ethylene-propylene rubber with high ENB (ethylidene norbornene) content and a high Mooney viscosity. The very low ethylene content ensures excellent low temperature properties. The very high Mooney viscosity and high ENB contributes to a high level of physical properties and very fast curing performances. This grade is very suitable fro automotive sponge applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³
Mooney Viscosity 60
@Temperature 150 °C
60
@Temperature 302 °F
(1+8); ISO 289
Storage Temperature >= 30.0 °C>= 86.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Content44 percentEthylene, ASTM D3900
 9 percentENB, ASTM D6047

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Keltan® 5465Q Ethylene-Propylene Rubber
Lanxess Keltan® 8550C Ethylene-Propylene Rubber
Lanxess Keltan® 5470Q Ethylene-Propylene Rubber
Lanxess Keltan® 6160D Ethylene-Propylene Rubber
Lanxess Keltan® 7752C Ethylene-Propylene Rubber

PLANY8601 / 208994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.