MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Brewer Science ProTEK® B3 Alkaline-Resistant Coating
Categories: Other Engineering Material

Material Notes: ProTEK® B3 coatings thin films are spin-applied polymeric coating systems that provide temporary wet-etch protection for CMOS MEMS circuitry during alkaline or acid etches. ProTEK® B materials offer protection from alkaline solutions such as KOH and TMAH for extended bath etches.
  • Protect delicate front-side circuitry during backside bulk micromachining
  • Increase yield by minimizing front-side damage caused by alkaline etch solution punch-through during wet etching
  • Improve throughput by reducing labor and process time associated with mechanical clamps and increasing the number of wafers per etch bath
The ProTEK® B3 Primer and ProTEK® B3 Protective Coating are applied separately. The film thickness can be varied through adjustment of spin speed. Suggested spin speeds are between 1000 rpm and 4000 rpm.

Information provided by Brewer Science.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 4.20 microns0.165 milSpin Speed 4000 rpm
 8.80 microns0.346 milSpin Speed 1000 rpm
 
Processing PropertiesMetricEnglishComments
Shelf Life  6.00 Month
@Temperature 16.0 - 26.0 °C
6.00 Month
@Temperature 60.8 - 78.8 °F
Primer
 12.0 Month
@Temperature 16.0 - 26.0 °C
12.0 Month
@Temperature 60.8 - 78.8 °F
Coating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brewer Science WaferBOND CR-220 Temporary Bonding Material
Brewer Science ProTEK® PSB Photosensitive Protective Coating
Brewer Science BrewerBOND® 701 Laser Release Material
Brewer Science BrewerBOND® 510 Temporary Bonding Material
Brewer Science BrewerBOND® 305 Temporary Bonding Material

PBREW994 / 193510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.