MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KEP Kepital® F25-03H Acetal Copolymer, Medium viscosity, High rigidity
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Medium-low viscosity grade with higher stiffness and strength than standard KEPITAL maintaining acetal copolymer's inherent characteristics.

Information provided by KEP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Water Absorption 0.20 %0.20 %ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/int = 3 mm
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 68.0 MPa9860 psi50 mm/min; ISO 527
Elongation at Break 32 %32 %50 mm/min; ISO 527
Elongation at Yield 10 %10 %50 mm/min; ISO 527
Flexural Strength 94.0 MPa13600 psiISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Strength 19.0 kV/mm483 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C66.7 µin/in-°FISO 11359
Melting Point 168 °C334 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KEP Kepital® F25-03 Acetal Copolymer, Medium viscosity
Network Polymers Kepital® F10-02
BLUESTAR BS025 Acetal Copolymer
BASF Ultraform® N2320 006 POM
Avient LubriOne™ AT-000/05T Acetal (POM) Copolymer

PKEP9946 / 185622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.