MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ArcelorMittal FB 590 Hot rolled ferrite-bainite steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Available in the following: uncoated (HDT590F)

Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: FB 450, 540, 560 and 590. This family of steels extends the HSLA range of micro-alloyed steels to include products combining high tensile strength (UTS) with excellent formability and hole expansion (stretch flangeability) based on their ferrite-bainite microstructure.

Applications: These steels are cold-drawn. The main applications are:

  • structural parts (longitudinal beams, cross beams, car-body and ground liason parts),
  • wheels,
  • mechanical parts (ground liason parts, gear boxes...).
ArcelorMittal has an extensive database relating to the forming and service properties of the entire range of ferrite-bainite steels. To integrate these steels at the design stage, a team of experts is available to perform specific studies based on modeling or laboratory tests.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 590 - 670 MPa85600 - 97200 psi
Tensile Strength, Yield 480 - 600 MPa69600 - 87000 psi
Elongation at Break >= 16 %>= 16 %L0=80 mm, th<3 mm
 >= 21 %>= 21 %L0=5.65v 0 mm, th<3 mm
Fatigue Strength  <= 490 MPa
@# of Cycles 2.00e+6
<= 71100 psi
@# of Cycles 2.00e+6
 <= 490 MPa
@# of Cycles 1.00e+7
<= 71100 psi
@# of Cycles 1.00e+7
 <= 550 MPa
@# of Cycles 100000
<= 79800 psi
@# of Cycles 100000
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Iron, Fe >= 98.15 %>= 98.15 %as balance
Manganese, Mn <= 1.6 %<= 1.6 %
Silicon, Si <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ArcelorMittal FB 590 HHE Hot rolled ferrite-bainite steel
Assab Steels 760 Machinery Steel
JIS S45C Steel, Normalized
AISI 1008 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 mm thick
Special Metals INCONELĀ® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, Solution Treated

NARCE036 / 159944

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.