MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® MP 2313 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on polyolefin substrates. Monprene® TPE gels are recommended for applications where very soft tactile feel and strength are required, such as cushions or padding between hard substrates and personal contact.

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.870 g/cc0.870 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 125 °C
10 g/10 min
@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM D2240
Tensile Strength at Break 1.24 MPa180 psiASTM D412
Tensile Stress at Strain 0.241 MPa
@Strain 300 %
35.0 psi
@Strain 300 %
ASTM D412
Elongation at Break 700 %700 %ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® MP 1870 Thermoplastic Elastomer
Teknor Apex Monprene® MP 2356 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1504 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer

PTEKNO734 / 128915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.