MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is available in both dark and light electrical Grey, other colors can be made upon request.

Benefits: The product offers a robust glow wire resistance, combined with enhanced processing behavior suitable for thin wall parts.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This product is ideally suited for power distribution applications such as MCB housing.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
Water Absorption 1.0 %
@Temperature 23.0 °C,
Time 86400 sec
1.0 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 275 °C
20 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO/FDIS 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psiISO 527 Type 1A
 75.0 MPa10900 psiASTM D638
Elongation at Break 3.0 %3.0 %ISO 527 Type 1A
 3.0 %3.0 %ASTM D638
Tensile Modulus 6.40 GPa928 ksiISO 527 Type 1A
Flexural Strength 130 MPa18900 psiASTM D790
 136 MPa19700 psiISO 178
Flexural Modulus 0.600 GPa87.0 ksiISO 178
 5.70 GPa827 ksiASTM D790
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inASTM D256
Charpy Impact Unnotched 4.70 J/cm²22.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 252 V252 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FISO 75/Af
 145 °C293 °FASTM D648
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
1210
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
1210
Oxygen Index 31 %31 %ISO 4589
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone230-240°C
Mixing Zone245-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ascend Performance Materials Starflam® PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Envalior Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond)
Domo TECHNYL® 2417IG PA66, 20% glass fiber, DRY
Domo TECHNYL® 2412GM05-D PA66, 38% glass fiber, DRY
Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY

PRHOD799 / 138030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.