MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product comes in 2-2.5 mm round pellets.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 - 0.740 g/cc0.0231 - 0.0267 lb/in³
Density 1.12 - 1.15 g/cc0.0405 - 0.0415 lb/in³
Moisture Absorption at Equilibrium 2.6 %2.6 %23°C/50% RH
Water Absorption at Saturation 9.5 %9.5 %23°C
Water Vapor Transmission 28.0 g/m²/day1.80 g/100 in²/day85% RH
Oxygen Transmission Rate 14.0 cc/m²/day0.902 cc/100 in²/day50% RH
Viscosity Measurement 3.49 - 3.713.49 - 3.71(RV) 1% [m/v] in 96% [m/m] sulfuric acid; ISO 307
 210 - 226210 - 226(RV) 0.5% [m/v] in 96% [m/m] sulfuric acid; ISO 307
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psiTD
 75.0 MPa10900 psiMD
Elongation at Break 380 %380 %MD
 400 %400 %TD
Tensile Modulus 0.650 GPa94.3 ksiMD
 0.700 GPa102 ksiTD
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 7.00e+14 ohm7.00e+14 ohm
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Melting Point 220 °C428 °F
Decomposition Temperature >= 300 °C>= 572 °F
Ignition Temperature >= 400 °C>= 752 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.060 %0.060 %ISO 15512
 
Descriptive Properties
Commercial StatusEurope
Extractables<0.6 %ISO 6427
Nucleating Agent250 - 550 mg/kgBASF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Thiodiglycol HP
BASF Ultramid® C33 01 PA66/6 (Conditioned)
BASF Ultramid® C33L 01 PA66/6 (Dry)
BASF Ultramid® C33 01 PA66/6 (Dry)
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE

PBASG0349 / 131982

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.