MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Avient Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Custom Molding

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccProperties reported for Natural color.; ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
Spiral Flow 58.4 cm23.0 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 797910 sec; ASTM D2240
Tensile Strength, Yield 46.2 MPa6700 psiType I, 51 mm/min; ASTM D638
Elongation at Break 50 %50 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2.24 GPa325 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 68.3 MPa9910 psiASTM D790
Flexural Modulus 2.28 GPa331 ksiASTM D790
Izod Impact, Notched  1.30 J/cm
@Thickness 3.18 mm,
Temperature -18.0 °C
2.44 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
Injection Molded; ASTM D256A
 6.40 J/cm
@Thickness 3.18 mm,
Temperature 0.000 °C
12.0 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
Injection Molded; ASTM D256A
 9.60 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
18.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy 89.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.167 ft-lb/mil
@Thickness 0.125 in,
Temperature 73.4 °F
Procedure A, 1/8-in. conical No brittle breaks. MFE/Avg. thk. > 264/0.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C77.8 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi)  77.3 °C
@Thickness 3.18 mm
171 °F
@Thickness 0.125 in
Injection Molded; Unannealed; ASTM D648
 82.0 °C
@Thickness 3.18 mm
180 °F
@Thickness 0.125 in
Injection Molded; Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  64.4 °C
@Thickness 3.18 mm
148 °F
@Thickness 0.125 in
Injection Molded; Unannealed; ASTM D648
 74.1 °C
@Thickness 3.18 mm
165 °F
@Thickness 0.125 in
Injection Molded; Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 210 °C390 - 410 °F
 
Descriptive Properties
AppearanceOpaque
FeaturesGeneral Purpose
 High Impact Resistance
 Medium Flow
FormsPellets
Generic MaterialPVC Alloy
Generic NamePolyvinyl Chloride Alloy (PVC Alloy)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 General Purpose
 Outdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Novablend™ 6602 Polyvinyl Chloride, Rigid
Avient Novablend™ 5035 Polyvinyl Chloride, Rigid
Avient Novablend™ 4578 Polyvinyl Chloride, Rigid
Avient Novablend™ 2677 Polyvinyl Chloride, Rigid

PH0POL1243 / 145812

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.