MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

3M Scotch-Weld™ MG100 SF Medical Grade Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plastics, rubbers, and composite materials and are available with special properties such as fast cure, low odor, flexibility and a variety of viscosities. This product has been tested and meets the specifications of USP Class VI. These products are not intended for use in implantable medical assemblies or for direct application to the skin. MG100 SF is a fast curing cyanoacrylates that rely less on surface moisture for cure speed than standard cyanoacrylates. These cyanoacylates can be used for a super fast cure in high speed production applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
Viscosity 80 - 120 cP80 - 120 cPISO 3104/3105
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.5 MPa3700 psicured, grit-blasted steel; ASTM D2095
Shear Strength 20.0 MPa2900 psiOverlap, grit-blasted steel; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °F
Minimum Service Temperature, Air -54.0 °C-65.2 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0500 - 0.500 min0.000833 - 0.00833 hourTime to Handling
 1440 min24.0 hourFull Cure
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
AppearanceClear Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ MG77 AC Medical Grade Instant Adhesive Primer
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive
3M Scotch-Weld™ MG79 AC Medical Grade Instant Adhesive Primer
3M Scotch-Weld™ MG20 SF Medical Grade Instant Adhesive

PMM34742 / 169489

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.