MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestamid® Terra DS 16 natural Nylon 1010
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: VESTAMID Terra DS16 natural color is a medium-viscosity PA 1010. VESTAMID Terra DS16 is semi-crystalline, which is the reason for its high mechanical resistance and chemical stability. It absorbs only little water. As a result its mechanical properties vary little when exposed to changing environmental humidity, and the material features a high dimensional stability. VESTAMID Terra DS16 can be used to manufacture transparent films. The high melting point of VESTAMID Terra DS16 compounds results in a high heat deflection temperature that can be advantageous for some applications. VESTAMID Terra DS16 occupies a position between the high-performance long-chain polyamides such as PA 12 and PA 1212 and the standard polyamides PA 6 and PA 66, which have a shorter chain length. Because of its chemical and physical properties, and the plant origin of its monomers, VESTAMID Terra DS16 is an interesting addition to conventional longer chain polyamides, and it also meets the growing demand for materials made from renewable raw materials. VESTAMID Terra DS16 natural color is supplied as cylindrical granules, ready for processing, in moisture-proof bags. VESTAMID® Terra DS is the polycondensation product of 1,10-decamethylene diamine (D) and 1,10-decanedioic acid (sebacic acid—S). Because both monomers are extracted from castor oil, VESTAMID® Terra DS is based on natural, renewable resources up to 100%.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Water Absorption at Saturation 1.8 %1.8 %ISO 62
Viscosity Number 160 cm³/g1.60 dl/gISO 307
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psiISO 527-1, ISO 527-2
Elongation at Break >= 50 %>= 50 %ISO 527-1, ISO 527-2
Elongation at Yield 5.0 %5.0 %ISO 527-1, ISO 527-2
Tensile Modulus 1.70 GPa247 ksiISO 527-1, ISO 527-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1/1 eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1/1 eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
complete break, incl. hinge break H; ISO 179-1/1 eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
complete break, incl. hinge break H; ISO 179-1/1 eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °F2nd heating, DSC; ISO 11357
Vicat Softening Point  171 °C
@Load 5.10 kg
340 °F
@Load 11.2 lb
Method B; ISO 306
 196 °C
@Load 1.02 kg
385 °F
@Load 2.25 lb
Method A; ISO 306
 
Descriptive Properties
Global Warming Potential (kgCO2 equivalent/kg material)2.8Evonik, PE International, preliminary data
Renewable Carbon (%)100ASTM 6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® Terra DS 18 natural color Nylon 1010
Evonik Trogamid® CX7323 Transparent Nylon
Evonik Trogamid® A4000 Transparent Polyamide
Evonik VESTAMID® NRG 1001 PA 12
Evonik Vestamid® Terra DD16 Nylon 1012

PEVONIK991 / 192754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.