MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mallard Creek Polymers Rovene® 6117 Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Applications: Rovene® 6117 is a clear drying, 100% acrylic, water resistant latex emulsion designed to provide protection for all types of concrete, cementitious and rigid surfaces. Rovene® 6117 features:
  • Efflorescence resistant
  • Good Durability
  • Resistance to blushing
  • Excellent resistance to a variety of chemicals
  • Highly water resistant
  • Very good adhesion
  • Protects against water penetration
  • Non-yellowing
Rovene® 6117 is a specialty acrylic emulsion designed for use in concrete sealing applications, but it can also be used in primers, deck coatings and pigmented masonry coatings. It can be formulated as a clear or a low %PVC pigmented coating. Depending on the selection of coalescing solvents, Rovene® 6117 can be formulated to less than 100 g/L VOC to comply with governmental regulations. Rovene® 6117 is the ideal choice to beautify and provide protection to patios, sidewalks, driveways, decking, garage floors, basements and concrete walls.

Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6117 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 47.5 - 48.5 %47.5 - 48.5 %
Particle Size 0.14 µm0.14 µm
pH 6.5 - 7.56.5 - 7.5
Brookfield Viscosity 50 - 250 cP50 - 250 cP#20/200
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.97 MPa285 psi
Elongation at Break 301 %301 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 30.0 °C86.0 °F
 
Descriptive Properties
EmulsifiersNonionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mallard Creek Polymers Rovene® 6104 Styrene-Acrylic Emulsion
Mallard Creek Polymers Rovene® 6126 Styrene-Acrylic Emulsion
Mallard Creek Polymers Rovene® 6119 Styrene-Acrylic Emulsion
Mallard Creek Polymers Rovene® 6112 Styrene-Acrylic Emulsion
Mallard Creek Polymers Rovene® 6111 Styrene-Acrylic Emulsion

PMCP103 / 157204

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.