MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® AKV 30 H3.0 000000 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: PA 66, 30% glass fibers, injection molding, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.9 %1.9 %50% RH; ISO 62
Water Absorption at Saturation 5.5 %5.5 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 1100 N
@Temperature 23.0 °C
247 lb (f)
@Temperature 73.4 °F
ISO 6603-2
Ball Indentation Hardness 130 MPa18900 psiISO 2093-1
Tensile Strength at Break 115 MPa16700 psi5 mm/min; ISO 527-1,-2
Elongation at Break 6.5 %6.5 %5 mm/min; ISO 527-1,-2
Tensile Modulus 6.00 GPa870 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 185 MPa26800 psi2 mm/min; ISO 178-A
Flexural Yield Strength 145 MPa
@Strain 3.5 %
21000 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 5.50 GPa798 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 6.0 %6.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  55.0 kJ/m²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 70.0 kJ/m²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Puncture Energy 4.20 J
@Temperature 23.0 °C
3.10 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °F10°C/min; ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °Finjection molding; ISO 294
 280 - 300 °C536 - 572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
Envalior Durethan® AKV 30 GIT H2.0 900116 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 30 GIT H2.0 900116 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Envalior Durethan® AKV 30 G HR DUS023 900116 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 30 G HR DUS023 900116 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned

PLANW9223 / 208020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.