MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Applications
  • Extrusion
  • Injection
  • Pneumatic Hose
  • Transparent Hose
  • Industry Parts

Information provided by API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9696ASTM D2240
Tensile Strength 49.0 MPa7110 psiASTM D412
Tensile Stress at Strain 14.7 MPa
@Strain 100 %
2130 psi
@Strain 100 %
ASTM D412
Elongation at Break 450 %450 %ASTM D412
Tear Strength 167 kN/m952 pliASTM D624
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 195 - 205 °C383 - 401 °FInjection Molding
Zone 1 160 - 175 °C320 - 347 °FInjection Molding
 160 - 175 °C320 - 347 °FExtrusion Molding
Zone 2 180 - 190 °C356 - 374 °FInjection Molding
 185 - 195 °C365 - 383 °FExtrusion Molding
Zone 3 180 - 195 °C356 - 383 °FExtrusion Molding
 185 - 195 °C365 - 383 °FInjection Molding
Zone 4 190 - 205 °C374 - 401 °FExtrusion Molding
Die Temperature 190 - 205 °C374 - 401 °FExtrusion Molding
Head Temperature 195 - 210 °C383 - 410 °FExtrusion Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® AC-4095A TPU – Clear Aromatic
Lubrizol LifeSciences Carbothane® PC-3555D TPU – Clear Aliphatic
Lubrizol LifeSciences Carbothane® AC-4055D-B20 Aromatic TPU
Lubrizol LifeSciences Carbothane® AC-4055D TPU – Clear Aromatic
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced

PKOKZ999 / 122701

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.