System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
MetalTek MTEK 20M Cast UNS J94650 Super Austenitic Stainless Steel
Categories:
Metal
;
Ferrous Metal
;
Austenitic
;
Stainless Steel
;
Cast Stainless Steel
Material Notes:
Corrosion resistance approaching nickel alloys, especially in chloride service.
Applications: Process piping exposed to flue gas and solutions.
Information provided by MetalTek
Key Words:
Cast UNS J94650; Cast Grade CN7MS; Cast ASTM A744
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
156
156
Tensile Strength, Ultimate
>=
485
MPa
>=
70300
psi
Tensile Strength, Yield
>=
205
MPa
>=
29700
psi
Elongation at Break
>= 35 %
>= 35 %
Component Elements Properties
Metric
English
Comments
Carbon, C
<= 0.070 %
<= 0.070 %
Chromium, Cr
18 - 20 %
18 - 20 %
Copper, Cu
1.5 - 2.0 %
1.5 - 2.0 %
Iron, Fe
45.43 - 53.5 %
45.43 - 53.5 %
As Balance
Manganese, Mn
<= 1.0 %
<= 1.0 %
Molybdenum, Mo
2.5 - 3.0 %
2.5 - 3.0 %
Nickel, Ni
22 - 25 %
22 - 25 %
Silicon, Si
2.5 - 3.5 %
2.5 - 3.5 %
Descriptive Properties
Heat Treatment
Sol. Anneal
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Cast Stainless Steel CN7MS, ASTM A744
Cast Stainless Steel CN7MS, UNS J94650
Crucible Steel SUE52 Martensitic Steel
Overview of materials for Austenitic
Carpenter Speed StarĀ® High Speed Steel (Red-Hard) (AISI M2)
NMETEK057 / 18307
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.