MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco HiPerSYN™ ISO 68 Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.

They provide outstanding thermal and oxidation stability, high viscosity index, high flash point, low pour point, and excellent hydrolytic stability.

Chevron HiPerSYN Oils protect against rust, oxidation, and foaming, and have good antiwear properties. The natural thermal and oxidation stability of these lubricants, due to their high level of purity and refinement, has been further enhanced by their unique additive systems.

The high thermal and oxidation stability reduces the formation of oxidation byproducts and acidic materials which will eventually cause deposits and varnish. They are able to withstand relatively high temperature operations for extended periods of time. They have very good demulsibility characteristics allowing quick release of moisture.

They minimize entrained air, which could otherwise result in reduced lubricant film thickness and potentially lead to pump cavitation.

Chevron HiPerSYN Oils pass the acute aquatic toxicity (LC-50) criteria adopted by the U.S. Fish and Wildlife Service and the U.S. Environmental Protection Agency (EPA). Chevron HiPerSYN Oils are registered with NSF and are acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.

Applications

Chevron HiPerSYN Oils are formulated to provide outstanding lubricating qualities for air compressors, especially portable and stationary rotary, vane, and screw compressors.

Chevron HiPerSYN Oils are recommended for industrial bearings and gears, such as worm gears, that require an R&O type synthetic gear oil.

Chevron HiPerSYN Oils are designed for applications with wide operating temperature ranges. They are especially effective in high temperature applications, like sootblowers, where outstanding thermal and oxidative stability are required.

Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed. Do not use in breathing air apparatus or medical equipment.

Key Words: CPS Number: 259138; MSDS Number: 8562
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 35.9 °35.9 °
Viscosity Measurement 150150Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 330 SUS330 SUS
Saybolt Viscosity at 210°F 61.7 SUS61.7 SUS
Kinematic Viscosity at 40°C (104°F) 64.6 cSt64.6 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 10.4 cSt10.4 cStASTM D445
Oxidative Stability 30 hour30 hour25 psi pressure drop; ASTM D2272
 >= 18000 hour>= 18000 hourHours to 2.0 mg KOH/g acid number; ASTM D943
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.410 mm0.0161 in1800 rpm
 
Thermal PropertiesMetricEnglishComments
Pour Point -42.0 °C-43.6 °FASTM D97
Flash Point 254 °C489 °FASTM D92
 
Descriptive Properties
ColorL 0.5
Corrosion, Copper Strip Test 3h1B
Foaming Stability, mL0
Foaming Tendency Sequence I10
Water Separability, Minutes to 0 mL emulsion15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Rheolub® RL-415 Wax Blend

WCHEV319 / 74934

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.