MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Main Characteristic:
  • Age hardening alloy
  • Beriyllium free alloy
  • Good machinability
  • High mechanical properties
Typical Applications:
  • Coaxial connectors
  • Spectacles parts
  • Sliding contacts parts
  • All kind of turned parts

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 220 - 240220 - 240
Tensile Strength, Ultimate 680 - 740 MPa98600 - 107000 psi
Tensile Strength, Yield 610 - 660 MPa
@Strain 0.2 %
88500 - 95700 psi
@Strain 0.2 %
Elongation at Break <= 4.0 %<= 4.0 %Alo 100 mm
Modulus of Rigidity 115 GPa16700 ksiTorsion
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000130 ohm-cm0.0000130 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.2 µm/m-°C
@Temperature 0.000 - 200 °C
9.56 µin/in-°F
@Temperature 32.0 - 392 °F
Thermal Conductivity 55.0 W/m-K382 BTU-in/hr-ft²-°F
Melting Point 960 °C1760 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 87 %87 %
Nickel, Ni 7.5 %7.5 %
Other 0.50 %0.50 %
Tin, Sn 5.0 %5.0 %
 
Descriptive Properties
ColorPinky roseate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy
CLAL-MSX DECLAFOR® 1015 TDX Wire quenched/Cold Rolled Copper Alloy
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy

NCLAL044 / 160075

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.