MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Norton® Fluorglas® Chemfilm® DF2929 Fluoropolymer Tape
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess superior dielectric properties. The multi-layer process is ideal for bulk and surface properties suited to most demanding applications.

DF2000 Series: Combines fluoropolymers with the highest temperature rating and the best electrical properties with the mechanical integrity and dielectric strength of polyimide film. Heat sealable surfaces allow these tapes to be sealed to itself and other layers of fluoropolymer tape wrap insulation at regular wire processing temperatures and the fully sintered fluoropolymer base resin enables the films to be wrapped directly over the conductor.

DF2919/DF2929 Performance: Test programs in both military and commercial aircraft markets indicate the benefits of a proper ratio between fluoropolymers and polyimides to give maximum protection against arc propagation and failure.

Applications include: Wire and Cable Industry Applications
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D-792
Water Absorption <= 0.25 %<= 0.25 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 145 MPa21000 psiASTM D-882
Elongation at Break 100 %100 %ASTM D-882
Tensile Modulus 2.41 GPa350 ksiASTM D-882
Tear Strength 500 kN/m2860 pliInitial Tear Strength; ASTM D-1004
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 3.80e+17 ohm3.80e+17 ohmASTM D-257
Dielectric Constant 2.8
@Frequency 60.0 - 1.00e+8 Hz
2.8
@Frequency 60.0 - 1.00e+8 Hz
ASTM D-150
Dielectric Strength 201 kV/mm5100 kV/inASTM D-149
Dissipation Factor 0.0130.013ASTM D-150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °FUL-746 B
Minimum Service Temperature, Air -240 °C-400 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medium-Silicon Ductile Iron, heat-resistant ductile iron
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron
Tra-Con Tra-Duct 2929 Room Temperature Conductive Flexible Silver Epoxy Adhesive
Celanese Hytrel® 8238 TPC-ET
Aclo Accutech Nylon 6 NY0730G20L Glass Reinforced

PSTGQZ151 / 68665

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.