MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potters Industries A-Series Premium 1.5MM Soda-Lime Silica Technical Quality Solid Glass Spheres
Categories: Ceramic; Glass

Material Notes: Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil drilling.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.53 g/cc0.0554 lb/in³
Density 2.50 g/cc0.0903 lb/in³
Particle Size 1300 - 1700 µm1300 - 1700 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 515
@Load 0.100 kg
515
@Load 0.221 lb
kg/mm²
Hardness, Mohs 5.0 - 6.05.0 - 6.0
Compressive Strength 96.5 - 248 MPa14000 - 36000 psi
Coefficient of Friction 0.90 - 1.00.90 - 1.0
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.51 - 1.521.51 - 1.52
 
Descriptive Properties
% Round90
Free Silica Content (%)0
Shapespherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries A100 Solid Glass Spheres
Potters Industries Ballotini® AAA Metal Finishing Glass Bead
Potters Industries Ballotini® Impact Beads
Potters Industries Premium 1.5 mm Solid Glass Spheres
Potters Industries SHERIGLASS® Type I Solid Glass Spacer Bead

CPOT9915 / 161905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.