Red-brown hexagonal crystals. Weathering end product(s): Limonite, ochre. Occurrence: Pigment in sediments. Hydrates slowly to limonite, rust burst. Property values are typical of naturally occurring Hematite (Fe2O3). Actual property values will vary from sample to sample. |